Reference Standard
CC331G-GC UNI EN 1982 | Chemical Analysis % Chemical Composition |
||||||||||||
Sn% | Zn% | Pb% | Fe% | Ni% | Al% | P% | Si% | Mn% | Sb% | As% | Cu% | Rest | |
Min | - | - | - | 1,50 | - | 8,50 | - | - | - | - | - | 83,00 | - |
Max | 0,20 | 0,50 | 0,10 | 3,50 | 1,50 | 10,50 | - | 0,20 | 1,00 | - | - | 89,50 | - |
Casting Process and Designation | Mechanical Properties | |||
Yield Strength Rp 0.2 N/mm² | Tensile Strength Rm N/mm² | Elongation at Break A% | Brinell Hardness HB |
|
Sand Cast -GS | 180 | 500 | 18 | 100 |
Shell Cast -GM | 250 | 600 | 20 | 130 |
Centrifugal Cast -GZ | 200 | 550 | 18 | 130 |
Continuous Cast -GC | 200 | 550 | 15 | 130 |
Application:
This standardized alloy is particularly suitable for chemical plants. In general mechanics, it is recommended for applications requiring high plastic properties.
Examples of application: mining water pumps, centrifugal pump impellers, lightly loaded ship propellers, bearings, valve seats and guides, helical gears, etc.