| Reference Standard
CC491K-GC UNI EN 1982 | Chemical Analysis % Chemical Composition |
||||||||||||
| Sn% | Zn% | Pb% | Fe% | Ni% | Al% | P% | Si% | Mn% | Sb% | As% | Cu% | Rest | |
| Min | 4,00 | 4,00 | 4,00 | - | - | - | - | - | - | - | - | 83,00 | - |
| Max | 6,00 | 6,00 | 6,00 | 0,30 | 2,00 | 0,01 | 0,10 | 0,01 | 0,20 | 0,25 | - | 87,00 | - |
| Casting Process and Designation | Mechanical Properties | |||
| Yield Strength Rp 0.2 N/mm² | Tensile Strength Rm N/mm² | Elongation at Break A% | Brinell Hardness HB |
|
| Sand Cast -GS | 90 | 200 | 13 | 60 |
| Shell Cast -GM | 110 | 220 | 6 | 65 |
| Centrifugal Cast -GZ | 110 | 250 | 13 | 65 |
| Continuous Cast -GC | 110 | 250 | 13 | 65 |
Application:
Alloy for general purposes.
N.B.: For further information, please contact our Sales Office